Hastelloy® Alloy X is a nickel-chromium-iron-molybdenum alloy that offers excellent oxidation resistance and strength at elevated temperatures.
성분 | UNS N06002 % |
니켈 | 47 balance |
크롬 | 22.00 |
철 | 18 |
몰리브덴 | 9.00 |
코발트 | 1.5 |
텅스텐 | 0.6 |
망간 | 1 max |
실리콘 | 1 max |
붕소 | 0.008 max |
나이오븀 | 0.50 최대 |
알루미늄 | 0.50 최대 |
타이태늄 | 0.15 max |
미터식 | 영어 | |
밀도 | 8.22 g/cm³ | 0.297 lbs/in³ |
Electrical resistivity | 17.87 µohms/cm | 45.4 µohms/in |
Thermal conductivity | 9.2 W/m °C | 63 Btu-in/ft²hr-°F |
*thermal conductivity at 25° C [75° F], electrical resistivity 25° C [75° F]
Cold worked % | Yield strength | Ultimate tensile strength | Elongation % |
0 | 427 MPa [62 ksi] | 827 MPa [120 ksi] | 38 |
20 | 1014 MPa [147 ksi] | 1165 MPa [169 ksi] | 5.8 |
37 | 1131 MPa [164 ksi] | 1303 MPa [189 ksi] | 3.9 |
50 | 1379 MPa [200 ksi] | 1558 MPa [226 ksi] | 3.1 |
60 | 1310 MPa [190 ksi] | 1627 MPa [236 ksi] | 2.4 |
All data represent results from a 25.4 cm [10 in] test gauge length. Values are typical and may not represent all diameters. Test method will affect results.